Preparación de películas delgadas de AS2S3 por depósito químico con perspectivas de aplicacíon en celdas solares
DOI:
https://doi.org/10.29105/qh1.1-52Keywords:
depósito quimico, celdas solares, películas delgadasAbstract
In this paper we obtained thin films of As2S3 by chemical bath deposition. The films were prepared at a temperature of 80 ºC for 3 hours each deposit. They were thermally treated at 180 ºC and 250 ºC for 30 minutes for 1 hour, respectively. The energy gap was calculated 2.9 eV. The conductivity was around, 3.62X10-1 (O*cmr'.
Downloads
References
-[1] L.P. Deshmukh, A.B. Palwe, V.S. Sawant, 1990, Solar Ce/Is, Volume 28, lssue 1, Pages 1-10 DOI: https://doi.org/10.1016/0379-6787(90)90033-2
-[2] Cimpl Z, Kosek F, and Lukes F 1987 J. Non-Cryst. Solids 97&98 439 DOI: https://doi.org/10.1016/0022-3093(87)90103-7
-[3] Dikova J and Starboa K 2000 Vacuum 58 490 DOI: https://doi.org/10.1016/S0042-207X(00)00210-4
-[4] White K, Kumar B, and Rai A K 1988 Thin Solid Films 147 275
-[5] Santiago J J, Sano M, Hamman M and Chen N 1987 Thin Solid Films 147 275 DOI: https://doi.org/10.1016/0040-6090(87)90023-X
-[6] Yesugade NS, Lokhandr CD and Bhosale CH 1995 Thin Solid Films, 263 145 DOI: https://doi.org/10.1016/0040-6090(95)06577-6
-[7] Sartale S D and Lokhande C D 2000 Mater. Res. Bul. 35 1345 DOI: https://doi.org/10.1016/S0025-5408(00)00330-5
-[8] Mane R S, sankapal B R and Lokhande CD 2000 Mater. Chem. and phys. 64 215 DOI: https://doi.org/10.1016/S0254-0584(99)00261-8
Downloads
Published
How to Cite
Issue
Section
License
Copyright (c) 2010 Y. Peña, A. Benitez, S. Lugo, P. Elizondo, T. Garza
This work is licensed under a Creative Commons Attribution 4.0 International License.